Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 185 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 178 - 185 °C
352 - 365 °F
Ordinary type
Oceanchem Group 1,2,5,6,9,10-Hexabromocyclododecane (HBCD)
Molecular Formula: C12H18Br6Cas No.: 3194-55-6Characteristics: The product is white crystalline powder, melting point greater than 180°C, bromine content greater than or equal to 73%. This product..
Melting Point 182 - 185 °C
360 - 365 °F
Oceanchem Group Antioxidant 168
Molecular Formula: C42H63O3PCas No.: 31570-04-4Characteristics and Uses: This product is an excellent antioxidant namely applied to polyethylene, polypropylene, polyoxymethylene, ABS resin, PS resin..
Melting Point 162 - 185 °C
324 - 365 °F
Average value: 167 °C Grade Count:19
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Melting Point 174 - 185 °C
345 - 365 °F
Average value: 178 °C Grade Count:14
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Melting Point 165 - 185 °C
329 - 365 °F
Average value: 176 °C Grade Count:27
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Melting Point 135 - 185 °C
275 - 365 °F
Huntsman/TMA
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi..
Melting Point 170 - 185 °C
338 - 365 °F
Huntsman/TMA
Huntsman IROGRAN® A 92 H 4656 Polyester-Based TPU-Injection Molding Grade
Introduction: IROGRAN A 92 H 4656 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are short cycle times, good melt flow and e..
Melting Point 125 - 185 °C
257 - 365 °F
ScanTube THV Tubing
Information provided by ScanTube, Inc.
Melting Point 173 - 185 °C
343 - 365 °F
Williams Advanced Alloys WS185 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Melting Point 120 - 185 °C
248 - 365 °F
Zeus THV Tubing
THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity.
Copyright © lookpolymers.com All Rights Reserved