| Category | Polymer , Thermoplastic , Fluoropolymer |
| Manufacturer | ScanTube |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | ScanTube THV Tubing.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.97 g/cc | 0.0712 lb/in³ | ASTM D792 |
| Water Absorption | <= 0.010 % | <= 0.010 % | ASTM D257 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 45 | 45 | ASTM D2240 |
| Tensile Strength | 29.6 MPa | 4300 psi | ASTM D638, ASTM D1708 |
| Elongation at Break | 500 % | 500 % | ASTM D638, ASTM D1708 |
| Tensile Modulus | 0.207 GPa | 30.0 ksi | ASTM D638 |
| Flexural Modulus | 1.24 GPa | 180 ksi | ASTM D790 |
| Compressive Strength | 12.4 MPa | 1800 psi | ASTM D695 |
| Izod Impact, Notched | NB | NB | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Thermal Conductivity | 0.202 W/m-K | 1.40 BTU-in/hr-ft²-°F | ASTM C177 |
| Melting Point | 125 - 185 °C | 257 - 365 °F | |
| Maximum Service Temperature, Air | 120 °C | 248 °F | Continuous |
| Deflection Temperature at 0.46 MPa (66 psi) | 31.0 - 37.0 °C | 87.8 - 98.6 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 28.0 - 32.0 °C | 82.4 - 89.6 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | >= 65 % | >= 65 % | ASTM D2863 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.5 @Frequency 1000 Hz |
3.5 @Frequency 1000 Hz |
ASTM D150 |
| 4.2 @Frequency 1.00e+6 Hz |
4.2 @Frequency 1.00e+6 Hz |
ASTM D150 | |
| Dielectric Strength | 0.709 kV/mm | 18.0 kV/in | Short Term; 10 mil film; ASTM D149 |
| Dissipation Factor | 0.12 @Frequency 1000 Hz |
0.12 @Frequency 1000 Hz |
ASTM D150 |
| 0.17 @Frequency 1.00e+6 Hz |
0.17 @Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Chemical Resistance | Good | |
| Weather Resistance | Excellent |