Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 224 °C | 435 °F | |
Plastcom SLOVASTER® B GF 40 PBT reinforced with 40% glass fibre Features: PBT for injection moulding, chemically reinforced with 40% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bendi.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
Nylene® 9543 , 43% Glass Reinforced Nylon 6/12 Description: Nylene® 9543 s a 43% glass fiber reinforced specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |
|||
Melting Point | 224 - 229 °C | 435 - 444 °F | |
Oceanchem Group Antioxidant 1024 Molecular Formula: C34H52N2O4Uses: Dosage is 0.1-0.5 portions. It is a metal deactivator, can work with antioxidant, used in PE, PP, polystyrene, polyamnamee, polyester, or used as antioxidant of b.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® SK612SF NC010 PBT
(Unverified Data**) Crastin® SK612SF is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PL471 45 Shore D, Injection Grade Copolyester Elastomer (North America)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G45 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP513FLBL Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Melting Point | 224 °C | 435 °F | |
Eastman Eastar DN007 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP212G15V0BM G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, paintabilityApplications: A variety of cases and connectorsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, high flowApplications: A variety of cases and connectorsInformation provided by API-Kolon. Information provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP212V0BLK Flame Retardant PBT Compound Resin Flame retardant, BLACKApplications: ConnectorsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G15HIBL Impact Resistant PBT Compound resin G/F 15% + Impact resistantApplications: SwitchesInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G30 Flame Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | ASTM D1525 |
Kolon SPESIN® KP270BL General Purpose PBT Compound Resin Excellent waterproofnessApplications: ConnectorsInformation provided by API-Kolon. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® BKV 30 FN00 000000 Nylon 6, 30% Glass Fiber PA6, injection molding grade, 30% glass fibers, UL94 V-0 at 0,75 mm , free of halogen and red phosphorus, glow wire flammability test max. 960°C |
|||
Melting Point | 224 °C | 435 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF20HI 20% Glass Fiber Reinforced, High Impact PBT Information provided by A. Schulman. |
|||
Melting Point | 224 °C | 435 °F | DSC Peak; JIS K7121 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S600F20 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 BK851 is an unreinforced lubricated medium viscosity black polybutylene terephthalate resin for injection molding.Information.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® S610SF BK851 Polybutylene Terephthalate (PBT) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin S610SF is an unreinforced low viscosity polybutylene terephthalate for injection molding. It has hig.. |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® SK612SF BK591 PBT Crastin® SK612SF BK591 is a 15% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast .. |
|||
Melting Point | 224 °C | 435 °F | ISO 3146 |
Azoty Tarnow™ Alphalon™ E 40 T Nylon 6 A bright polyamide 6 grade of medium viscosity that is suited for the production of films and monofilaments.Information provided by ATT Polymers™ |
|||
Melting Point | 224 °C | 435 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® PL471 Polyether Ester Elastomer (European Grade)
(discontinued **) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melting Point | 224 °C | 435 °F | DIN 53736; ASTM D789 |
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |