Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 129 °C | 264 °F | Internal method |
Polimeri Europa Eraclene® FB 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3417 |
NOVA Chemicals Novapol® TI-0338-A MDPE Masterbatch Resin Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3417 |
NOVA Chemicals Sclair® 35BE HDPE Extrusion Resin
(discontinued **) Features: Medium molecular weight HDPE, excellent ESCR, excellent toughness, good processability, outstanding abrasion resistance.Applications: Extrusion on to metal pipes to produce a corrosion res.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3418 |
ExxonMobil HD 6510 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3418 |
ExxonMobil HD 6510.17 Injection Molding Resin
(discontinued **) HD 6510 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a wide ra.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total Finathene® 1288 HDPE film
(discontinued **) Applications: Flat bottom bags, draw strings, coextruded merchandise bags, deli wrapInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plasti.. |
|||
Melting Point | 129 °C | 264 °F | ISO 3146 |
Total Lacqtene® 2001 PBK 44 HDPE pipe
(discontinued **) LACQTENE® 2001 PBK 44 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 PBK 44 is a black compound especially developed for s.. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3417 |
NOVA Chemicals Novapol® TR-0338-U MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Melting Point | 129 - 133 °C | 264 - 271 °F | |
Hong Kun Group UV Absorber Chemical Name: 2-(2'-Hydroxy-5'-methylphenyl)benzotriazoleCAS No. 2440-22-4All information provided by Hongkun Group |
|||
Melting Point | 129 - 142 °C | 264 - 288 °F | TMA Melt Range |
Huntsman IROGRAN® PS 455-215 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 129 °C | 265 °F | |
Heatbath/Park Scale Kleen 1259 Descaling Salt A highly alkaline and oxidizing salt bath used specifically as a low temperature bath for descaling titanium and titanium alloys.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Melting Point | 129 °C | 264 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 4164 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total 6410 HDPE Film Resin Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw.. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3417 |
Total 8183 HDPE, blow molding Applications: cosmetic bottles, pharmaceutical bottles, industrial product containers, chemical packaging, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals ac.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE 6280 High Density Polyethylene, Injection Molding Resin Characteristics:Excellent stiffnessExcellent surface appearanceGood warp resistanceExcellent impact resistanceASTM D 1248 - Type III, Class A, Category 3FDA CompliantApplications:Dairy cratesPallets.. |
|||
Melting Point | 129 °C | 264 °F | DSC-2 Differential Scanning Calorimeter |
Total PPR Z9450 Random Copolymer Heat Sealable Grade ATOFINA Z9450 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The very low melting point of ATOFINA Z9450 makes it an excellent heat seal layer f.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE 6480 High Density Polyethylene, Clarity Cast Film Resin Polyethylene: Clarity High Density Cast Film ResinCharacteristics:High stiffnessHigh clarityExcellent surface glossHigh tensile strengthGood barrier propertiesLow gel contentApplications:OverwrapFo.. |
|||
Melting Point | 129 °C | 265 °F | ASTM D3417 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Melting Point | 129 °C | 264 °F | Dow Method (DSC) |
Dow ASPUN™ 6835A Linear Low-Density Polyethylene (LLDPE) ASPUN™ 6835A Fiber Grade Resin: Suggested Optimum Process: Staple CardableTypical Application: Yarn & Bonding FibersInformation provided by Dow |
|||
Melting Point | 129 °C | 264 °F | ASTM D3418 |
ExxonMobil HD 6733.17 Injection Molding Resin Product Description: HD 6733 is a narrow molecular weight hexane copolymer designed to maximize injection molding speed and productivity in thing wall articles. Lower processing temperatures enable .. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3418 |
ExxonMobil HD 8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3418 |
ExxonMobil HDP8660.29 Rotational Molding Resin Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o.. |
|||
Melting Point | 129 °C | 264 °F | Exxon Method |
ExxonMobil Escorene® HD-7745 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7745 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Melting Point | 129 °C | 264 °F | Exxon Method |
ExxonMobil Escorene® HD-7755 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7755 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Melting Point | 129 °C | 264 °F | Exxon Method |
ExxonMobil Escorene® HD-7756 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HD-7756 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Melting Point | 129 °C | 264 °F | Exxon Method |
ExxonMobil Escorene® HDZ-123 HMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high molecular weight HDPE blown film resin. Films made from HDZ-123 exhibit excellent impact and toughness properties as well as high stiffness... |
|||
Melting Point | 129 °C | 264 °F | ASTM D3417 |
Total Finathene® RS 528 HDPE blow molding
(discontinued **) Applications: Bleach and detergents, industrial chemicals, industrial parts, cosmetic bottles, food packaging.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Melting Point | 129 °C | 264 °F | |
Total Lacqtene® 2001 TN 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TN 46 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2001 TN 46 is used for sewage pipe, smooth protective condu.. |
|||
Melting Point | 129 °C | 264 °F | ASTM D3417 |
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin
(discontinued **) Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer. |
|||
Melting Point | 129 °C | 264 °F | Internal method |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |