Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
CTE, linear, Parallel to Flow | 50.0 - 60.0 µm/m-°C @Temperature 50.0 - 100 °C |
27.8 - 33.3 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 1-7313 000000 PBT + PET, 15% Glass Fiber PBT+PET, 15% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1100F PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be supported with b.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem MD130A PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, ISO 10993 compliant in recognized colors.This data was supplied by SABIC-IP for the Europe-.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
27.8 µin/in-°F @Temperature -58.0 - 122 °F |
1 |
Solvay Specialty Polymers Ryton® QC220P Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 150 °C |
27.8 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM AUT200M PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C) with internal mold release.. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are re.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-15/2 PA6-GF15 Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Rilsan® AZM 30 NOIR T6LD Nylon 12, 30% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-060,GF30Rigid grade with glass fiber (30%) for injection molding. Available color: black. Reinforced light and heat stabilizing agent. Mold-release agent.High rigid.. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced PBT-GF10Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 50.0 µm/m-°C @Temperature 20.0 °C |
27.8 µin/in-°F @Temperature 68.0 °F |
|
BASF Procom® D 1158 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 50.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
CTE, linear, Parallel to Flow | 50.0 - 60.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 33.3 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |