Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 3404 33% Glass Reinforced SMC Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required... |
|||
CTE, linear, Parallel to Flow | 35.0 - 40.0 µm/m-°C @Temperature 50.0 - 150 °C |
19.4 - 22.2 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K224-HGR24 Nylon 6-30% Glass Fiber and Glass Bead Reinforced (European Grade) (Dry)
(discontinued The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ASTM D696 |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications:.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MFB63 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFB63 is a compound based on Polypropylene resin containing Glass Bead, Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® TV4 260 SN PBT-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)
(Unverified Data**) 25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RFB24 PA66, 20/10% Glass Fiber/Glass Bead Filled Injection Molded RFB24 is a Glass Bead and Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as Staramide 66 2010VK Z3)Information provided by Polymer Technology & Services, the North American.. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 20.0 °C |
19.4 µin/in-°F @Temperature 68.0 °F |
|
BASF Luranyl® KR 2403 G6 Polyphenylene Ether + Styrene-Butadiene Blend, 30% Glass Fiber Reinforced General-purpose grade with 30% glass fiber for parts requiring especially good resistance to heat deformation.Applications: parts for hot-water contact, pump housings, fan blades.Data was collected .. |
|||
CTE, linear, Parallel to Flow | 35.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® V9230CS PET (Europe-Africa-Middle East) 15% GF PET Injection Moulding grade, Heat and Color Stabilised, for light colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |