Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -20.0 - 150 °C |
11.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -20.0 - 150 °C |
11.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® ABS CF30 BK 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PPS 05002 Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementFeatures: Electrically ConductiveInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 GF33 FR-N BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame Retardant and Halogen FreeAppearance: BlackInformation provided by TP Composites, Inc... |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 CF30 30% Carbon Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF18 HS L 18% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 18% Filler by Weight Additive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedInformat.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF20 HS L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Additive: Lubricant and Heat StabilizerFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF20 L 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF20 L BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing: Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF20 L UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6 GF20 RM BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Features: Low Moisture AbsorptionAppearance: BlackInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 E GF33 LE 33% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightFeatures: Low ExtractablesProcessing Method: ExtrusionInformation provided by TP Composi.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GB40 HS BK 40% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: BlackInforma.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 L BKN001 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 NAT001 Y 33% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PC GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS GF/M65 BK 65% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 65% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS/F GF/M35 X 35% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PC CF15 TL6 BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, I.. |
|||
CTE, linear, Parallel to Flow | 19.8 - 30.6 µm/m-°C @Temperature -20.0 - 150 °C |
11.0 - 17.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PS+PA (Asia Pacific) GR 30%. Highest stiffness of 1200000 psi (8200 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: under the bonnet. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6 CF30 TL10 30% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant(10%)Features: Conductive and LubricatedAppearance: BlackInform.. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
11.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PPA GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, High Heat Resistance and Low .. |
|||
CTE, linear, Parallel to Flow | 19.8 µm/m-°C | 11.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6 E CF20 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightFeatures: Conductive Appearance: Natural ColorProcessing Method: ExtrusionInformation p.. |