| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) |
| Manufacturer | ATG s.r.l. |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | ATG s.r.l. ACM Polyacrylic Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.11 g/cc | 1.11 g/cc |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 50 - 90 | 50 - 90 | |
| Tensile Strength, Ultimate | 5.00 - 14.0 MPa | 725 - 2030 psi | |
| Elongation at Break | 100 - 350 % | 100 - 350 % | |
| Rebound | 5.0 - 8.0 % | 5.0 - 8.0 % |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 170 °C | 338 °F | |
| Minimum Service Temperature, Air | -20.0 °C | -4.00 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Abrasion Resistance | low | |
| Chemical Resistance to Animal and Vegetable Oils and Greases | high | |
| Chemical Resistance to Aromatic Hydrocarbons | none | |
| Chemical Resistance to Chloride Solvents | none | |
| Chemical Resistance to Distilled Water | low | |
| Chemical Resistance to Ketones | none | |
| Chemical Resistance to Maximum Concentrated Alkalis (at 50°C) | low | |
| Chemical Resistance to Medium-High Concentrated Acids (at 50°C) | low | |
| Chemical Resistance to Mineral Oils and Aliphatic Hydrocarbons | high | |
| Compression set at 100°C | high | |
| Impermeability at gas (Oxygen and Nitrogen) | medium | |
| Resistance to Flame | none | |
| Resistance to Heat Aging | high | |
| Resistance to Low Temperatures | low | |
| Resistance to Ozone and Weathering | high | |
| Tear Strength | low |