Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Manifattura Cattaneo RULON® 641 Polytetrafluoroethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Garlock GRAPH-LOCK® 3123/3125 Graphite Sheet Gasketing A pure graphite sheet. Thicknesses |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Garlock GRAPH-LOCK® 3125TC Graphite Sheet Gasketing, Steel Insert A laminated graphite sheet with a 316SS tang insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSeals e.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Garlock GRAPH-LOCK® 3128 HOCHDRUCK® Graphite Sheet Gasketing, Steel Reinforced High performance multi-layer graphite with 316SS inserts provides high compressive strength, blow-out resistance, excellent handling properties and improved tightness.Pure exfoliated graphite flake .. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded .. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
GrafTech GRAFOIL® GHL Standard Fluid Sealing Grade GHL Laminate GRAFOIL® Grade GHL is a laminate made with GRAFOIL® Grade GTB flexible graphite. Laminate thicknesses > 0.060" will be adhesively bonded to final thickness. Laminate thicknesses |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1700 Heat Bondable PTFE Film Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE Rulon® 1337 is a tan material made entirely from FDA compliant components. It has excellent physical properties and is chemically compatible with most chemicals, except concentrated sulfuric acid.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for .. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® 641 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® 945 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | Embrittlement Temp |
Saint-Gobain Rulon® 954 Bearing/Seal PTFE A conductive PTFE material that is available in tape, sheet (extruded) and rod (extruded).Information provided by distributor TriStar Plastics Corp. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® 957 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | Embrittlement Temp |
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | Embrittlement Temp |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2919 Fluoropolymer Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2929 Fluoropolymer Tape Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® 142 Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Saint-Gobain Rulon® AR Bearing/Seal PTFE Rulon® AR is somewhat more flexible than Rulon® LR, hence suitable for seals and bonded coating of slide surfaces. It has many decades of use in automotive shaft seals and fuel metering pump c.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
XADC-Armoloy Diamond-Chrome Composite Coating XADC-Armoloy® combines the Armoloy® TDC chromium coating with spherical diamond particulates. The XADC-Armoloy® coating enhances the durability of components used in a wide range of applications.. |
|||
Minimum Service Temperature, Air | -240 - -200 °C | -400 - -328 °F | |
Zeus FEP Tubing FEP, fluorinated ethylene propylene, is a melt processable fluoropolymer that allows for long, continuous lengths and has several distinct advantages over PTFE. Applications where FEP tubing is usua.. |
|||
Minimum Service Temperature, Air | -240 °C | -400 °F | |
Chesterton Valvelon® 3500 PTFE Sealant Description: Chesterton® 3500 Valvelon® is a dense, pure PTFE sealant that can be used as a non-hardening valve packing or flange gasket. The unique construction of the product allows it to squeez.. |