Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film

Category Polymer , Film , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Norton® Fluorglas® Chemfilm®
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess superior dielectric properties. The multi-layer process is ideal for bulk and surface properties suited to most demanding applications.DF1700/1900 Series: These films have a PTFE core with a thin layer of FEP or PFA (DF1700P) on one surface, which makes them heat bondable. Double bondable (DB) films are also available with PFA on both surfaces or FEP on one surface and PFA on the other surface. Laser markable (LM) films are also available. PTFE = polytetrafluoroethyleneApplications include: Wire and Cable Industry ApplicationsInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D-792
Water Absorption <= 0.010 %
<= 0.010 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.6 MPa
4300 psi
ASTM D-882
Elongation at Break 400 %
400 %
ASTM D-882
Tensile Modulus 0.414 GPa
60.0 ksi
ASTM D-882
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
UL-746 B
Minimum Service Temperature, Air -240 °C
-400 °F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Surface Resistivity per Square 1.00e+18 ohm
1.00e+18 ohm
ASTM D-257
Dielectric Constant 2.0

@Frequency 60.0 - 1.00e+8 Hz
2.0

@Frequency 60.0 - 1.00e+8 Hz
ASTM D-150
Dielectric Strength 165 kV/mm
4200 kV/in
ASTM D-149
Dissipation Factor >= 0.00010
>= 0.00010
ASTM D-150