Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 623B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 952 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | continuous |
Orbilan RubberLen® R70 TPE, light grey ORBILAN RUBBERLEN® is a two-layered laminated panel made from Thermoplastic Elastomer (TPE) and low-pressure Polyethylene of High Molecular Weight (HMW-PE). RUBBERLEN® distinguishes itself by very.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering E70X Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Rubber, 65-75 °IRHD. Copolymer of ethylene and propylene.Applications: Excellent water and steam resistance with good compression set properties. Superior heat a.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering N70L Nitrile Rubber Nitrile Butadiene Rubber (NBR), 70 °IRHD. Low- Med acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet: ASTM D2000/SAE J200 line call-out: M5BG710, A14, B14, EO14, EO34.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering C50M Chloroprene Rubber Chloroprene Rubber, 46-55 °IRHD. Formulated to meet British Standard BS2752 grade C50.Applications: A versatile rubber with good compression set properties, giving moderate resistance to petroleum.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® HPC 1300 Unsaturated Polyester UP HPC 1300 is a special SMC for high strength applications. The glass level has been selected to combine mouldability with high strength and stiffness properties in orientation direction. The reinforc.. |
|||
Minimum Service Temperature, Air | <= -40.0 °C | <= -40.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1410-t1 Polyolefin TPO Granules, Grey Lucofin are colored, highly stabilized polyolefin-based TPO granules. The t1 series is distinguished by good tenacity, high biaxial extensibility and flexibility outstanding breaking strength, and .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 1200 Cast Polyamide 12, Dry Application: sprockets, chain-wheels, pulleys, wheels, slide and seal rings, curve disks, etc.Information provided by Schwartz Technical Plastics GmbH |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 317 Cast Polyamide 6, Heat Stabilized, Conditioned Application: coupling parts, sealing rings, bearingsInformation provided by Schwartz Technical Plastics GmbH |
|||
Minimum Service Temperature, Air | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
SMAC SMACWRAP® EX Damping Material, 0.12 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | See Note 1. |
ChevronTexaco Multifak® AFB NLGI Grade 2 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | See Note 1. |
ChevronTexaco Polystar® Synthetic 4602 NLGI Grade Texaco Polystar Synthetic 4602 delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -40°C to 230°C (-40°F to 446°F) and offers ex.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
3M 4000 UV 6586 Marine Adhesive/Sealant Fast Cure 3M™ Marine Adhesive/Sealant 4000 UV is a one-part adhesive sealant that cures to form a firm, rubbery waterproof seal. Its flexibility allows for the dissipation of stress caused by shock, vibratio.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
3M Scotchcal™ ElectroCut™ 413 Graphic Film Product Description:3.25 mil cast film in 6 glossy, opaque, fluorescent colorExtremely conspicuous in daylight and activated by exposure to near ultraviolet light (but not black light)Offers high at.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
ATG s.r.l. EPM Ethylene-Propylene Copolymer |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
3M 5200 Marine Adhesive/Sealant Fast Cure A fast curing, one-part polyurethane that chemically reacts with moisture to deliver strong, flexible bonds with excellent adhesion to wood and fiberglass. Forms watertight, weather-resistant seals .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7908 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Parker Chomerics CHO-FOIL CAD Shielding Tape Conductive Adhesive Aluminum FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Alcoa KAMA 1500 Freezer Modified OPS
(discontinued **) CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coati.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® EP1199 Black Unfilled Epoxy Adhesive Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® UR3001HP Clear Urethane Encapsulant Resinlab™ UR3001HP Clear is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR3001HP Clear provides excellent e.. |