Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 368AX-L (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 748 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Recommended |
Nye Lubricants 786B (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | impact conditions and heavy loads not considered |
Omnia Plastica ABS Acrylonitrile-butadiene-styrene Acrylonitrile-butadiene-styrene is an amorphous thermopolymer used largely for injection moulded items. The stock shapes are mainly used for the production of prototypes.Features:Good machinability .. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V75X Fluoroelastomer Compound Graphite incorporated, Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out M2HK710, A1-10, B37, B38, EF31, EO78, F15, Z.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering V90W Fluoroelastomer Compound Off-White Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. Formulated using only those ingredients determined by the United States Food and Drug Admin.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering Z75R Hydrogenated NBR Compound Red Hydrogenated Nitrile Rubber, 70-80 °IRHD. Medium acrylonitrile (ACN) content. ASTM designation = HNBR. ASTM D2000 line call-out 2MDH708, A26, B36, EO16, EO36, F14, Z1. Z1 = hardness 75 ±5.Ap.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Precision Polymer Engineering Z80B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Rubber, 75-80 °IRHD. Medium acrylonitrile content (ACN = 33.5%). ASTM designation = HNBR. ASTM D2000 line call-out 4MDH716, A26, B36, EO16, EO36, F14, Z1. Z1 .. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Parker Chomerics CHO-BOND 1086 Conductive Caulk/Sealant Chomerics two-component conductive epoxy caulks provide excellent adhesion to dissimilar substrates and can be used in lap or butt joint applications. They feature large silver-plated-copper particl.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Manifattura Cattaneo PET Polyethylene Terephthalate Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Freudenberg Simrit V169 Fluoroelastomer Self-Lube Additives to elastomer compounds can improve the lubricity or non-stick performance of a seal. Specific compound ingredients may include fluoropolymer (TEFLON) additives, silicone additives or molyb.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Freudenberg Simrit V177 Fluoroelastomer Self-Lube Additives to elastomer compounds can improve the lubricity or non-stick performance of a seal. Specific compound ingredients may include fluoropolymer (TEFLON) additives, silicone additives or molyb.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Continuous |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Greene Tweed CHEMRAZ® SD625 Perfluoroelastomer Chemraz® SD625, a black-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resistance a.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Continuous; DIN 52612 |
Isoflon PETP Polyethylene terephthalate Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucobit® 1210 Ethylene Copolymer Bitumen Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Greene Tweed CHEMRAZ® 656 Perfluoroelastomer Chemraz® 656 is a low durometer perfluoroelastomer primarily designed for Bonded Slit Valve gates and special engineered applications such as low sealing forces/tolerance stickups where softer ma.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Trelleborg Z800 Commercial SBR Rubber Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Trelleborg Emerson & Cuming Stycast® G-508-1 One-Component Epoxy Flame Retardant Encapsulant Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conduc.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | |
Trelleborg Commercial Neoprene® C801 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | TR test, TR10 |
Daikin DAI-EL G-671 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 67% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Excellent low-temperature sealing .. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | JIS-K-6723 |
Denka VINYKON M7100 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | ASTM D 3575 |
Eurofoam Siliconcell 414/0 Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -20.0 °C | -4.00 °F | DSC |
Adamas Adalon® 206 PTFE, 15/5% Glass/MoS2 Filled Information provided by Adamas, HPM |