Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 1001 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants UniFlor 8160 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants UniFlor 8520 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Flex TR10; ASTM D1329 |
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Flex TR10; ASTM D1329 |
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer Flame Retardant Conductive Silicone Elastomer. CHO-SEAL 6370 EMI gaskets are conductive elastomers engineered for use in commercial electronic equipment where a high degree of flame retardancy and c.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Parker Chomerics CHO-SEAL® E6434E Conductive EPDM Elastomer Extruded Conductive EPDM Elastomer. This is an extruded conductive elastomer engineered for resistance to harsh chemicals, specifically those associated with decontaminates for military Nuclear, Bio.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Flex TR10 |
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer Description: Good performance in moderately corrosive environments; excellent NBC fluid resistance; good physical properties.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Cured |
Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive This multi-functional product is a rapid setting structural adhesive. UV-MX 2212 provides high impact, resilient bonds to many similar and dissimilar substrates. Multi-functional cure bonds are form.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; EN 495-5 |
Lucobit Lucofin® 1413 Polyolefin TPO Granules, Dark Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Master Bond MasterSil 707FR Flame Retardant Silicone Adhesive Description: MasterSil 707FR is a one component, high performance RTV silicone that is mainly used for its flame retardancy. It is UL listed with a flame classification for 94V-1 for thicknesses of .. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Trelleborg R642 Commercial Natural Rubber Polyisoprene All information provided by Trelleborg |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Retraction Temperature, TR10; ASTM D1329 |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with No Plasticizer MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 4445 CV KIT Two-part, grey, 1:1, addition cure gel, good thermal conductivity, controlled volatility, UL V-0.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning SE 4448 CV KIT PARTS A&B Excellent thermal conductivity, low volatility (D4-D10 0.03% wt), heat cure, high viscosity.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | JIS-K-6723 |
Denka REOMER G G3000 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | ASTM D 3575 |
Eurofoam Siliconcell 411/PLT Platinic Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning 3-4130 DIELECTRIC GEL KIT Two-part, clear, heat cure, low extractables.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
Dow Corning 3-4237 DIELECTRIC FIRM GEL KIT Two-part, translucent green, heat cure, firm, long working time, primerless chemical adhesion.Information provided by Dow Corning |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
ATG s.r.l. IR Synthetic Polyisoprene |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
ATG s.r.l. NR Natural Rubber |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | |
ATG s.r.l. XNBR Carboxylated Nitrile Rubber |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Recommended |
Nye Lubricants 2000F (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucofin® 1410MB Polyolefin TPO Granules, Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Minimum Service Temperature, Air | <= -45.0 °C | <= -49.0 °F | Low Temperature Flexural Test; DIN 53361 |
Lucobit Lucolit® 1320 Polyolefin TPO Granules, Beige Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi.. |
|||
Minimum Service Temperature, Air | -45.0 °C | -49.0 °F | Low Temperature Flexibility |
Sylvin Technologies 6147-83 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |