Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow Corning 3-4130 DIELECTRIC GEL KIT

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3-4130 DIELECTRIC GEL KIT.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part, clear, heat cure, low extractables.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
CTE, linear 440 µm/m-°C
244 µin/in-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.90e+14 ohm-cm
2.90e+14 ohm-cm
Dielectric Constant 2.88

@Frequency 100 Hz
2.88

@Frequency 100 Hz
2.88

@Frequency 100000 Hz
2.88

@Frequency 100000 Hz
Dielectric Strength 18.5 kV/mm
470 kV/in
Dissipation Factor <= 0.00010

@Frequency 100000 Hz
<= 0.00010

@Frequency 100000 Hz
0.0010

@Frequency 100 Hz
0.0010

@Frequency 100 Hz
Processing Properties Metric English Comments
Cure Time 4.00 min

@Temperature 150 °C
0.0667 hour

@Temperature 302 °F
5.50 min

@Temperature 125 °C
0.0917 hour

@Temperature 257 °F
7.50 min

@Temperature 100 °C
0.125 hour

@Temperature 212 °F
2880 min

@Temperature 22.0 °C
48.0 hour

@Temperature 71.6 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance clear
Flowable yes
Gel Hardness (Grams/Penetration) 155
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) 330
Users viewing this material also viewed the following: