Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 590 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 723F6 (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 758G (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Recommended |
Nye Lubricants 760D (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Continuous |
Nylacast H.S. Blue Cast Nylon 6, Heat Stabilized HS Blue is a heat Stabilised Cast Nylon 6. Its mechanical properties are maintained when operating at higher temperature and improves mechanical properties. This helps to reduce the stress distortio.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Precision Polymer Engineering B60B Styrene Butadiene Rubber Styrene-Butadiene Rubber (SBR) 55-65 °IRHD. Copolymer of styrene and butadiene.Applications: Good sealing resistance to brake fluids and water. Poor against petroleum oils, solvents and weather. .. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering N70M Nitrile Rubber Nitrile Butadiene Rubber (NBR), 68-78 °IRHD. Copolymer of acrylonitrile and butadiene. To meet BS2751 BA70 and ASTM D2000/SAE J200 line call-out 2MBG 714, B14, EA14, EF11, EF21, EO14, EO34, F17.Ap.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering N70W Nitrile Rubber White Nitrile Butadiene Rubber (NBR), 66-75 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administra.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering N70X Nitrile Rubber Self-lubricating, Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. Special fillers incorporated to enhance operation in dynamic sealing applications.Applicati.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Non-brittle after 3 minutes |
Precision Polymer Engineering R60R Natural Rubber Natural Rubber & Kevlar® NR6F722, 55-65 °IRHD. ASTM D1418 designation: NR. Kevlar® is a registered trademark of DuPont. ASTM D2000/SAE J200 Type, Class: AA.Applications: Natural rubber offers l.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 0390 Unsaturated Polyester UP BMC 0390 is a low profile DMC/BMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surface qua.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 0400 Unsaturated Polyester UP BMC 0400 is a low profile DMC/BMC for automotive applications. It fulfills the requirements of the automotive industry regarding painted body panels including reduced C-emissions. For highest surfac.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Continuous |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Dry Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Silikony Polskie Silpasta R Silicone Paste Semi-liquid consistencyLubricant agent during assembly of PVC pipelines. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg Neoprene® C423 Chloroprene CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Trelleborg Emerson & Cuming Stycast® 926-82-1 One-Component Epoxy High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Dow Corning MOLYKOTE® 822M GREASE Phenyl-methyl silicone grease for automotive brake boostersInformation provided by Dow Corning |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
3M 755 Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | Service |
3M 7735FL Acrylate Overlaminating Film 3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers exc.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Arlon 99-108065 PTFE Resin Design/Construction: Side 1: PTFESubstrate: Style 1080 Fiberglass Side 2: PTFE ResinAppearance: Brown Woven FabricThis data represents typical values for the production material. The data should not.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |
|||
Minimum Service Temperature, Air | -40.0 °C | -40.0 °F | |
Chesterton 635 SXC Synthetic, Extreme Pressure & Corrosion Resistant Grease Description: Chesterton® Synthetic Extreme Pressure & Corrosion Resistant Grease is the one grease to use for the most demanding lubricating needs. It is a multi-purpose workhorse with outstanding .. |