3M 7735FL Acrylate Overlaminating Film

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 7735FL Acrylate Overlaminating Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
3M™ Acrylate Overlaminating Film 7735FL utilizes an outdoor durable acrylate film facestock with exceptional UV resistance, combined with 3M™ Adhesive 400 and a film liner. This product offers excellent clarity and provides at least five years of outdoor life, when used with 3M™ Polyester Label Stocks, as explained belowInformation provided by 3M
Physical Properties Metric English Comments
Thickness 20.3 microns
0.800 mil
Adhesive
38.1 microns
1.50 mil
Liner
76.2 microns
3.00 mil
Facestock
Mechanical Properties Metric English Comments
Peel Strength 0.20817 kN/m
1.1875 pli
Polypropylene, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
0.20817 kN/m
1.1875 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.27391 kN/m
1.5625 pli
Stainless Steel, 180° Peel, Initial 10 min dwell at RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 79.0 °C
174 °F
Service
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Service
-12.0 °C
10.4 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type #400 Acrylic
Liner Clear Polyester Liner