Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate Information provided by Ravago |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1010G10FRMA Polycarbonate, 10% Glass Filled Polycarbonate, 10% Glass Filled, Flame RetardantInformation provided by Ravago. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1010L Polycarbonate, Unreinforced, Intermediate Flow Information provided by Ravago. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1017L Polycarbonate, Unreinforced, High Flow, Mold Release Information provided by Ravago. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1025L Polycarbonate, High Flow, Mold Release Information provided by Ravago |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1310L Polycarbonate, UV Stabilized, Intermediate Flow, Mold Release Information provided by Entec. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1317L Polycarbonate, UV Stabilized, Higher Flow, Mold Release Information provided by Ravago. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |
|||
Vicat Softening Point | 154 °C | 310 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1325L Polycarbonate, UV Stabilized, High Flow, Mold Release Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 900 Clear Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 910 Utility Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 920 Black Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 930 White Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 930-05V0 White Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 980 Grey Polycarbonate Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman 980-05V0 Grey Polycarbonate Glass Filled Easy processability, heat resistance, weatherability, color stability, self extinguishing5% glass fiber for foam moldingInformation provided by Shuman Plastics, Inc. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman FR910V0 Utility Black Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Shuman FR980V0 Grey Polycarbonate Flame Retardant Good impact strength, easy processability, good surface gloss, good heat resistance, excellent weatherability, excellent color stability, self extinguishingInformation provided by Shuman Plastics, I.. |
|||
Vicat Softening Point | 154 °C | 310 °F | |
Ensinger Tecanat™ Unfilled Polycarbonate (PC) Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps.. |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Entec Hylex® P1010L2 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and Medium Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Entec Hylex® P1017L1 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Clear/Transparent Information provided by Entec |
|||
Vicat Softening Point | 154 °C | 310 °F | ASTM D1525 |
Entec Hylex® P1017L2 HB Polycarbonate Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec |