Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 91.0 °C | 196 °F | 50 N - 50°C/h; ISO 306/B |
Polimeri Europa Edistir N 2560 Polystyrene High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble.. |
|||
Vicat Softening Point | 91.0 °C @Load 1.00 kg |
196 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FF 24 Low Density Polyethylene - Blown Film Extrusion Riblene FF 24 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 24 is characterized by a good melt s.. |
|||
Vicat Softening Point | 91.0 °C @Load 1.00 kg |
196 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CM6140 PC+ABS (Europe-Africa-Middle East) Cycoloy resin grade CM6140 is a flame retardant, filled PC/ABS blend. It is of non-brominated & non-chlorinated FR system to meet UL94 V0 at 0.8mm. Key features include thin wall FR, higher stiffnes.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | 50°C/h 10N; ISO 306 |
Yparex 8207 Polyolefin Adhesive Resin (European Grade)
(discontinued **) The Yparex range provides outstanding adhesion for all forms of polyethylene including cross-linked PE to: barrier plastics like EVOH and Polyamidemetals like aluminum, steel and copper.Yparex offer.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B; ASTM D1525 |
Ineos Nova PS 2521 Crystal Polystyrene
(discontinued **) Information provided by Nova ChemicalsINEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | DIN 53460 |
Ineos Nova S-6600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene which is very easy processed in extension and thermoforming processes. Typical applications are packaging of food stuffs like Yot beakers but technical parts and extruded pr.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | |
Eastman Tenite 358-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 17% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 18% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Vicat Softening Point | 91.0 - 245 °C | 196 - 473 °F | Average value: 130 °C Grade Count:32 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Vicat Softening Point | 91.0 °C @Load 5.00 kg |
196 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Vicat Softening Point | 91.0 °C @Load 5.00 kg |
196 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Vicat Softening Point | 91.0 °C | 196 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® GC-0703 ABS/PET, Unreinforced Recycled Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VE-0813 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | B (50 N); ISO 306 |
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | ASTM D1525 |
Dow AFFINITY™ PT 1409 Polyolefin Plastomer (POP) AFFINITY™ PT 1409 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies from Dow Plastics. Resin blended with 20 wt% LDPE to improve extrusion coating performance.Information provided b.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | |
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | 50°C/hr; 50N |
Arkema Group Appryl® HXN 1240 Polypropylene, 40% Talc Filled Compound of a PP homopolymer and 40% talc, warm stabilized suitable for under hood automotive applications.ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | ASTM D1525 |
Braskem EB 861/51 LDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Coextruded films; Shrink films for pallets; general purpose. Information provided by Brask.. |
|||
Vicat Softening Point | 91.0 °C @Load 1.02 kg |
196 °F @Load 2.25 lb |
ISO 306 |
Carmel Olefins IPETHENE® 830 Low Density Polyethylene IPETHENE® 830 is a low density polyethylene injection molding grade. It exhibits high melt flow rate and high stiffness. APPLICATIONS IPETHENE® 830 is used to produce lids, containers, toys, and.. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Vicat Softening Point | 91.0 °C | 196 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics XYLEX X8300CL PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester, UV Stabilized, Transparent, OQ Quality |
|||
Vicat Softening Point | 91.0 °C | 196 °F | ISO 306A |
Ineos Nova 205 Crystal Polystyrene General Purpose Grade
(discontinued **) Easy flow, Good mechanical property balance, Extrusion and Injection MoldingApplications: Sheet and film extrusion, Gloss capping, Blending with HIPS or SBSProperties were determined on injection m.. |