Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 75.0 °C | 167 °F | ISO 306 |
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Vicat Softening Point | 75.0 °C @Load 1.00 kg |
167 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Greenflex® FF 35 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 35 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. The resin shows good strechability and sealability.Main Applications: Greenflex FF 35 is suitable for flexibl.. |
|||
Vicat Softening Point | 75.0 - 108 °C | 167 - 226 °F | Average value: 95.5 °C Grade Count:98 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Vicat Softening Point | 75.0 °C @Load 1.00 kg, Thickness 4.00 mm |
167 °F @Load 2.20 lb, Thickness 0.157 in |
ISO 306 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Vicat Softening Point | 75.0 - 129 °C | 167 - 264 °F | Average value: 114 °C Grade Count:11 |
Overview of materials for High Density Polyethylene (HDPE), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | |
LyondellBasell Lupolen® 5231 HX HDPE, Impact Grade Medium flow, impact resistant, very stress-crack resistant grade for closures, bottles that contain carbonated liquids, storage and tote boxes, as well as engineering components.Data was collected b.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ISO 306 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5056 500 Micron LDPE Powder Description: ICOFLO 510-5056 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5058 1200 Micron LDPE Powder Description: ICOFLO 510-5058 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
ICO Polymers ICOTEXâ„¢ 520-5056 500 Micron LDPE Powder Description: ICOTEX 520-5056 is a low density polyethylene powder that has been developed to meet the special requirement of the textile coating industry. Key Characteristics: very high flow, very g.. |
|||
Vicat Softening Point | <= 75.0 °C | <= 167 °F | |
JPJ Technologies LD 150 LDPE Virgin Applications: Used for heavy duty packaging, packaging bags, general film bag, etc.Information provided by JPJ Technologies |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lushan M-20A Adhesive Resin for Multi-layer Oxygen Barrier Pipe Adhesive resin Lushan series for multi-layer oxygen barrier pipe is a modified polyolefin with functional groups. It’s designed to bond to a variety of barrier materials, such as nylon and ethy.. |
|||
Vicat Softening Point | >= 75.0 °C | >= 167 °F | ASTM D 1525 |
Karina E 835-18/115-C-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | 75.0 °C @Load 5.00 kg |
167 °F @Load 11.0 lb |
|
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler. UL94 V-0 classified, with brominated flame retardantsAvailability: Africa & Middle East; Asia Pacif.. |
|||
Vicat Softening Point | 75.0 °C @Load 5.00 kg |
167 °F @Load 11.0 lb |
|
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ISO 306B |
Lucite International Elvakon® 4461 Medium Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 870A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lubrizol Estane® T465A Thermoplastic Polyurethane Type: Estane® T465A is a Shore 71A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lubrizol Estane® CR185A Thermoplastic Polyurethane Type: Estane® CR185A is a Shore 85A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | B/50; ISO 306 |
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer Description: Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.Application: For all kinds of injection molded parts.Information provided by T.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | B (50N); ISO 306 |
Borealis Xmod™ PC75 High Crystalline Polypropylene Copolymer Xmod PC75 is a HCPP intended for injection molding of automotive interior parts. Xmod PC75 is a very easy-flowing material combined with a good balance between impact strength and stiffness. The m.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
DuPont Nucrel® 1202HC Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 11.5 wt% Methacrylic Acid.Nucrel® 1202HC (High-Clarity) is an ethylene-methacrylic acid copolymer resin available for use in conventional blown and cast film extrusion and coextrusion equipment des.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ISO 306 |
ExxonMobil LDPE LD 654 Low Density Polyethylene Resin (European Grade) Product Description: LD 654 is a very high flow LDPE grade with a very good flexibility. It can be added to low-flowing LDPE grades to improve their processability.Availability: Africa & Middle East.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ISO 306 |
Arkema Group OREVAC® 18921A Epoxide Modified Polyethylene OREVAC® 18921A is epoxide modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 18.. |
|||
Vicat Softening Point | 75.0 °C @Load 1.02 kg |
167 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem TN2005 EVA General Film Copolymer TN2005 is an Ethylene-Vinyl Acetate (EVA) copolymer with high molecular weight, excellent mechanical properties, transparency, high gloss, and easy processing. Additionally, TN2005 has flexibility e.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | B/120; ISO 306 |
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled SAXALEN PPC339T20 is a 20% mineral filled Polypropylene - Copolymer intended for injection molding with good flow properties und higher stiffness. The PP-Copolymer has low warpage behaviors and good.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
Lushan M-8D Adhesive Resin for Coextruded Multi-layer Barrier Packaging Film Adhesive resin Lushan series for multi-layer barrier food packaging film has durable bonding properties when adheres to Polarity materials, such as PE, PP and PA, EVOH, etc. Adhesive resin Lushan se.. |
|||
Vicat Softening Point | 75.0 °C | 167 °F | ASTM D1525 |
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |