Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 177 °C @Load 5.10 kg |
351 °F @Load 11.2 lb |
50°C/h |
Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Medium Modulus, Nominal Shore D/15s 50. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 175 PBT Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 176 PBT Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® 176HP PBT Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Vicat Softening Point | >= 177 °C | >= 350 °F | |
Master Bond UV15SP-1 Low Viscosity, UV Curable System Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea.. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r.. |
|||
Vicat Softening Point | 177 °C | 351 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif.. |