Polymer Property : Vicat Softening Point = 177 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 177 °C

@Load 5.10 kg
351 °F

@Load 11.2 lb
50°C/h
Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. Medium Modulus, Nominal Shore D/15s 50. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Vicat Softening Point 177 °C
351 °F
Rate B/50; ISO 306
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East)
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors.
Vicat Softening Point 177 °C
351 °F
Rate B/50; ISO 306
SABIC Innovative Plastics ULTEM DU319 PEI
Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East)
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 176 PBT
Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® EH7025AG PBT+PET
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Vicat Softening Point 177 °C
351 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Vicat Softening Point 177 °C
351 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
Vicat Softening Point 177 °C
351 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® IQ3001 PBT
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® IQ3001 PBT
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Vicat Softening Point >= 177 °C
>= 350 °F
Master Bond UV15SP-1 Low Viscosity, UV Curable System
Description: Master Bond UV15SP-1 is a new one component, high strength UV curable epoxy resin based polymer system for bonding, sealing, & coating with high performance properties. It is a 100% rea..
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
Vicat Softening Point 177 °C
351 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..