Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 149 °C | 300 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/h |
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
Vicat Softening Point | 149 °C | 300 °F | ASTM D1525 |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1201-10 Polycarbonate Resin Description: LUPOY PC 1201-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1301V-10 Polycarbonate Resin Description: LUPOY PC 1301V-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1300-12 Polycarbonate Resin Description: LUPOY PC 1300-12 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® L-1250Y Standard (mold release/ice color grade) Polycarbonate Resin Standard injection molding grade that has an improved mold release property and is bluish-tinted to exhibit clear color.Applications:Components of mechanical, electric, electronic, medical, safety a.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4330-10 Polycarbonate EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LV-2250Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required for normal fluidity.Applications:.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/h 50N; ISO 306 |
Covestro Makrolon® 3106 Polycarbonate ISO 7391-PC,M,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable.. |
|||
Vicat Softening Point | 149 °C | 300 °F | ISO 306/A50 |
ExxonMobil PP7011L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets .. |
|||
Vicat Softening Point | 149 °C | 300 °F | ASTM D1525 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXG154 PC (Asia Pacific) FXG154 is a Lexan PC grade with the Diamond effect. Color Package may affect properties, Application testing always recommended. |