Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.0 MPa @Temperature 175 °C |
5080 psi @Temperature 347 °F |
ISO 178 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Flexural Strength | 35.0 MPa @Strain 9.00 % |
5080 psi @Strain 9.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® B 40 SK 000000 Nylon 6 PA 6, non-reinforced, injection molding |
|||
Flexural Strength | 35.0 MPa @Strain 6.10 % |
5080 psi @Strain 6.10 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 35.0 MPa @Temperature 23.0 °C |
5080 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.9%); ASTM-D790 |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 35.0 MPa @Temperature 80.0 °C |
5080 psi @Temperature 176 °F |
Practical Use (Water Absorption 1.7%); ASTM-D790 |
Toyobo GLAMIDE® NB-5550 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 35.0 MPa @Temperature 23.0 °C |
5080 psi @Temperature 73.4 °F |
ASTM D790 |
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |
|||
Flexural Strength | 35.0 MPa @Strain 6.10 % |
5080 psi @Strain 6.10 % |
ISO 178 |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66