Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 21.0 kN/m | 120 pli | ISO 34-1 |
PolyOne OnFlex™ S EF 40A-3S1964 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ISO 34-1 |
PolyOne OnFlex™ S KG 60A-3S2018 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die B,post cured- 2 hours at 177°C; ASTM D624 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 21.0 kN/m | 120 pli | ASTM D624 |
Multibase Multi-Flex® A 4710 S Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Tear Strength | 21.0 kN/m | 120 pli | Warp/Longitudinal direction |
Saint-Gobain Chemlam® 6 Value Industrial Laminate Description: The Chemlam® series is the Chemfab® value line of industrial laminates. Chemlam® composites features uniform thickness, multi-layer cast PTFE films laminated to fiber glass rei.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Fill/Transverse direction |
Saint-Gobain COHRlastic® 1010 General-Purpose Electrical-Grade Silicone Coated Fabric Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 5 Anti-Static PTFE-Coated Glass Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electri.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® 6 Anti-Static PTFE-Coated Glass Description: Chemfab® Anti-static Series is a high quality PTFE-coated glass fabric that can be used for release sheets, belting, or other applications requiring the dissipation of static electri.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Tensile Strength (Warp) |
Saint-Gobain Chemfab® SlipGrip™ 6 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C; ASTM D624 |
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C; ASTM D1004 |
Teknor Apex TEKRON® 4000-60 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 21.0 kN/m | 120 pli | |
Dow Corning SILASTIC® 3496 MOULD MAKING BASE & 96 CURING AGENT High strength, low hardness, fast cure silicone mold making rubber featuring a very good resistance to polyester resin and suited for the detailed reproduction of fiines, art objects and similar ite.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Method C; ISO 34 |
ELASTO UK Dryflex® 3039-201 TPE, Modified Injection Molding Grade for Sanitary Seals The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3039-201 is specifically designe.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die B; silicone property; ASTM D624 |
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Tear Strength | 21.0 kN/m | 120 pli | [ppiw], Silicone Property; ASTM D624 |
Arlon 56344R025 0.025" (0.635 mm) Semi-cured Silicone Rubber Design/Construction: Interleave: PolyethyleneSide 1: Semi-Cured Silicone Rubber Substrate: 1564 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ISO 34-B |
AlphaGary Evoprene™ 047 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | [ppiw], Silicone Property |
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | ISO 34-B |
AlphaGary Evoprene™ GC 5656 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3850E Thermoplastic Elastomer - SBC
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tear Strength | 21.0 kN/m | 120 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58311 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Flat Die/Cast Film Extrusion, Profile ExtrusionAv.. |