Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
+/- 0.02; ASTM D792
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Yield 8.83 MPa
1280 psi
ASTM D412
Elongation at Break 725 %
725 %
ASTM D412
100% Modulus 0.00138 GPa
0.200 ksi
ASTM D412
Flexural Modulus 0.0324 GPa
4.70 ksi
ASTM D790
Tear Strength 21.0 kN/m
120 pli
Die C; ASTM D1004