Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.01962 GPa @Temperature 1500 °C, Time 10800 sec |
2.846 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories CTC-65SH Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 1000 °C, Time 10800 sec |
2.846 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 110 °C, Time 86400 sec |
2.846 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 110 °C, Time 86400 sec |
2.846 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-18 Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 110 °C, Time 86400 sec |
2.846 ksi @Temperature 230 °F, Time 24.0 hour |
|
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 1500 °C, Time 10800 sec |
2.846 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories MMCT-75 Special Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 1400 °C |
2.846 ksi @Temperature 2550 °F |
|
Chosun Refractories SB50 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 250 °C |
2.846 ksi @Temperature 482 °F |
|
Chosun Refractories SB75 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.01962 GPa @Temperature 1000 °C, Time 10800 sec |
2.846 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories SFC-70 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |