| Category | Ceramic , Carbide |
| Manufacturer | Chosun Refractories |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Chosun Refractories SFC-70 SiC Castable.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Modulus of Rupture | 0.00981 GPa <br>@Temperature 110 °C,<br> Time 86400 sec |
1.42 ksi <br>@Temperature 230 °F,<br> Time 24.0 hour |
|
| 0.01962 GPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
2.846 ksi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
||
| 0.024525 GPa <br>@Temperature 1350 °C,<br> Time 10800 sec |
3.5571 ksi <br>@Temperature 2460 °F,<br> Time 3.00 hour |
||
| Compressive Strength | 52.0 MPa <br>@Temperature 110 °C,<br> Time 86400 sec |
7540 psi <br>@Temperature 230 °F,<br> Time 24.0 hour |
Cold Crushing Strength |
| 88.3 MPa <br>@Temperature 1000 °C,<br> Time 10800 sec |
12800 psi <br>@Temperature 1830 °F,<br> Time 3.00 hour |
Cold Crushing Strength | |
| 118 MPa <br>@Temperature 1350 °C,<br> Time 10800 sec |
17100 psi <br>@Temperature 2460 °F,<br> Time 3.00 hour |
Cold Crushing Strength |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 1700 °C | 3090 °F | limited |
| Shrinkage | -0.150 % <br>@Temperature 1350 °C,<br> Time 10800 sec |
-0.150 % <br>@Temperature 2460 °F,<br> Time 3.00 hour |
|
| -0.0900 % <br>@Temperature 1000 °C,<br> Time 10800 sec |
-0.0900 % <br>@Temperature 1830 °F,<br> Time 3.00 hour |
||
| -0.0300 % <br>@Temperature 110 °C,<br> Time 86400 sec |
-0.0300 % <br>@Temperature 230 °F,<br> Time 24.0 hour |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Al2O3 | 18 % | 18 % | |
| SiC | 73 % | 73 % |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Installation Method | Self Flowing | |
| Material Required for Estimating(kg/?) | 2,610 | |
| Water Required for Casting(%) | 7.3-7.7 |