Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.002943 - 0.007848 GPa @Temperature 1350 °C, Time 10800 sec |
0.4269 - 1.138 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.003924 - 0.007848 GPa @Temperature 1350 °C, Time 10800 sec |
0.5691 - 1.138 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HACT-170 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 - 0.007848 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 - 1.138 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PT-160 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.004905 - 0.007848 GPa @Temperature 1500 °C, Time 10800 sec |
0.7114 - 1.138 ksi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories PT-165 Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.002943 - 0.007848 GPa @Temperature 1000 °C, Time 10800 sec |
0.4269 - 1.138 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HACT-150S High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |