Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.024525 GPa @Temperature 1000 °C, Time 10800 sec |
3.5571 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 1000 °C, Time 10800 sec |
3.5571 ksi @Temperature 1830 °F, Time 3.00 hour |
|
Chosun Refractories HSC-18RA Dense and High-Strength Castable, Superdense Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 250 °C |
3.5571 ksi @Temperature 482 °F |
|
Chosun Refractories SB50 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 250 °C |
3.5571 ksi @Temperature 482 °F |
|
Chosun Refractories SC80 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 1400 °C |
3.5571 ksi @Temperature 2550 °F |
|
Chosun Refractories SC80 Bricks, Oxide Bonded SiC Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 1350 °C, Time 10800 sec |
3.5571 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories SFC-70 SiC Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 1400 °C, Time 10800 sec |
3.5571 ksi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories SFC-90W High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Modulus of Rupture | 0.024525 GPa @Temperature 1350 °C, Time 10800 sec |
3.5571 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories SFC-UL90S High-Alumina Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |