Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.30 - 2.50 GPa | 334 - 363 ksi | ASTM D790 |
Prodways PLASTCure ABS 3650 3D Printing Polymer Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accur.. |
|||
Flexural Modulus | 1.90 - 2.50 GPa | 276 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8210 Rigid Opaque Prototyping Polymer Primary material: VeroBlueSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the .. |
|||
Flexural Modulus | 1.50 - 2.50 GPa | 218 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | 1.50 - 2.50 GPa | 218 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | 1.50 - 2.50 GPa | 218 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | 1.50 - 2.50 GPa | 218 - 363 ksi | ASTM D790-04 |
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Modulus | 1.90 - 2.50 GPa | 276 - 363 ksi | ASTM D790-04 |
Proto3000 Objet VeroBlue FullCure840 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Flexural Modulus | 0.00800 - 2.50 GPa @Temperature -40.0 - 100 °C |
1.16 - 363 ksi @Temperature -40.0 - 212 °F |
Average value: 0.758 GPa Grade Count:10 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 2.06 - 2.50 GPa @Temperature 60.0 - 120 °C |
299 - 363 ksi @Temperature 140 - 248 °F |
Average value: 2.26 GPa Grade Count:2 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 2.00 - 2.50 GPa | 290 - 363 ksi | ASTM D790 |
Loxim 810 01 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |