Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Proto3000
Trade Name Objet Digital Materials™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide the desired mechanical properties and to resemble the product’s target materials.Information provided by Proto3000 for their protoyping engineering services.
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 - 60.0 MPa
5800 - 8700 psi
ASTM D638-03
Elongation at Break 15 - 25 %
15 - 25 %
ASTM D638-05
Modulus of Elasticity 1.70 - 2.30 GPa
247 - 334 ksi
ASTM D638-04
Flexural Strength 55.0 - 75.0 MPa
7980 - 10900 psi
ASTM D790-03
Flexural Modulus 1.50 - 2.50 GPa
218 - 363 ksi
ASTM D790-04
Izod Impact, Notched 0.220 - 0.350 J/cm
0.412 - 0.656 ft-lb/in
ASTM D256-06
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Users viewing this material also viewed the following: