Polymer Property : Flexural Modulus = 3500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.14 - 24.1 GPa
600 - 3500 ksi
Average value: 9.97 GPa Grade Count:52
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Flexural Modulus 3.80 - 24.1 GPa
551 - 3500 ksi
Average value: 9.61 GPa Grade Count:155
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Flexural Modulus 2.00 - 24.1 GPa
290 - 3500 ksi
Average value: 7.17 GPa Grade Count:230
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Modulus 2.60 - 24.1 GPa
377 - 3500 ksi
Average value: 12.5 GPa Grade Count:29
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Flexural Modulus 2.41 - 24.1 GPa
350 - 3500 ksi
Average value: 13.0 GPa Grade Count:18
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..
Copyright © lookpolymers.com All Rights Reserved