Flexural Modulus 14.0 - 16.0 GPa
2030 - 2320 ksi
Injection and Compression; ISO 178
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Flexural Modulus 14.0 - 16.0 GPa
2030 - 2320 ksi
Injection and Compression; ISO 178
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
Flexural Modulus 12.0 - 16.0 GPa
1740 - 2320 ksi
Injection; ISO 178
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Flexural Modulus 13.0 - 16.0 GPa
1890 - 2320 ksi
Compression; ISO 178
Raschig Group RALUPOL® 4385 UP
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very high arc resistance, very high mechanical values. This product meets the allowed upper limits for heavy..
Flexural Modulus 13.0 - 16.0 GPa
1890 - 2320 ksi
Injection; ISO 178
Raschig Group RALUPOL® 4806 UP
Glass-fiber reinforced polyester molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values, better performance values compared to UP 80..
Flexural Modulus 14.0 - 16.0 GPa
2030 - 2320 ksi
Injection; ISO 178
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Flexural Modulus 14.0 - 16.0 GPa
2030 - 2320 ksi
Injection; ISO 178
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Flexural Modulus 13.0 - 16.0 GPa
1890 - 2320 ksi
Injection; ISO 178
Raschig Group SURAPLAST 54 UPA
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
Flexural Modulus 8.00 - 16.0 GPa
1160 - 2320 ksi
Average value: 12.5 GPa Grade Count:9
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Flexural Modulus 13.0 - 16.0 GPa
1890 - 2320 ksi
Injection; ISO 178
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
Flexural Modulus 5.52 - 16.0 GPa
800 - 2320 ksi
Average value: 9.57 GPa Grade Count:34
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Flexural Modulus 12.0 - 16.0 GPa
1740 - 2320 ksi
ISO 178
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound
Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat..
Copyright © lookpolymers.com All Rights Reserved