Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.86 GPa | 850 ksi | Tangent; ASTM D790 |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N2040MHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Polymer Resources NY6-M40-[color]-H Nylon 6, 40% Mineral Filled, Heat Stabilized Nylon 6, 40% Mineral Filled, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
PolyOne Edgetek® AS-20GF/000 HI UV NAT Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)& Description/Features:Glass Fiber ReinforcedHigh ImpactUV StabilizedNaturalUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | Tangent; ASTM D790 |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES Electrafil® M-2426 BK Polycarbonate |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES HiFill® PET 0268 B1 Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF004AH ABS LNP THERMOCOMP* AF004AH is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Techmer ES Luriblend® PSU GF20 TL5 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP SF006 PA 12 LNP THERMOCOMP* SF006 is a compound based on Nylon 12 resin containing 30% Glass Fiber. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS LNP* THERMOCOMP* AF004 is a compound based on ABS resin containing 20% Glass Fiber. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Chase Plastics CP Pryme® A220G ABS Molding Resin, 20% Glass Fiber Reinforced Information provided by Chase Plastics. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1244 Mineral Filled, General Purpose Polypropylene DescriptionPolyfort® FPP 1244 is a 40% mineral filled general purpose polypropylene for parts requiring ultra high stiffness, heat resistance and strength.Information provided by A. Schulman. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Ensinger Tecatron® XP-84 Compression Molded PPS Compound, 30% Graphite Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Clariant PA123G30 Nylon 66, 30% Glass Fiber, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Asahi Kasei Thermofil N-40MF-1600 40% Mineral Filled, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Aaron Industries AAROPRENE® MFN 6601 Mineral Filled Nylon 6/6 AAROPRENE® GFN & MFN 6600 Series Reinforced CompoundsColor may be specified. |
|||
Flexural Modulus | 5.86 GPa | 850 ksi | ASTM D790 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |