Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ASTM D792
Filler Content 30 %
30 %
Mechanical Properties Metric English Comments
Tensile Strength 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 0.30 %
0.30 %
ASTM D638
Flexural Strength 33.1 MPa
4800 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.262 J/cm
0.490 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color Black