Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne Nymax™ GF 600 A 14 Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1213HL BK Nylon 6/6 Available in North America Filler: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedRoHS CompliantForm: Pellets Proces.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne Edgetek® PK-1000 Polyetheretherketone (PEEK)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PK-5GP/7T Polyetheretherketone (PEEK), PTFE Lubricated
(discontinued **) Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Quadrant EPP Duratron® PAI T4501 Polyamide-imide, compression molded bearing grade (ASTM Product Data Sheet) |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
PTS Trimid® N66-G13LU 13% Glass Fiber Reinforced Utility Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 4.48 - 12.4 GPa | 650 - 1800 ksi | Average value: 7.74 GPa Grade Count:10 |
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Techmer ES HiFill® PA6 GF/B20 A2 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformation .. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02841 PBT+PC LNP* Thermocmop* 9X02841 is a PBT/Polycarbonate blend containing proprietary fillers. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
A. Schulman SCHULADUR® A GB30 30% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1080 Glass Fiber-Reinforced Homopolymer Polypropylene DescriptionPolyfort® FPP 1080 is a 20% fiber-reinforced homopolymer polypropylene with excellent strength and heat resistance. Information provided by A. Schulman. |
|||
Flexural Modulus | 4.48 GPa | 650 ksi | ASTM D790 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |