Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L4857 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Network Polymers Nylon 6609 Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Oxford Polymers Polysulfone PSF P170-64170 White PSU Product Description: Polysulfone injection molding grade, precolored white Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Continuous use up to 300(f)Informatio.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Niche Polymer PA66BK Nylon 66 Information provided by Niche Polymer |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL4016 PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer, for increased stiffness with good impact strength. Improved release properties. Available in limited colors only.This data was supplied by S.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PTS Trimid® N6-200N Nylon 6 with Nucleating Agent Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
PolyOne LubriOne™ ATH-000/05T Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1200HL BK Nylon 6/6
(discontinued **) Available in North AmericaAdditive: Heat Stabilizer and Lubricant Features: Lubricated and Heat StabilizedAuto Specifications: DELPHI QMPL-1257 Color: BlackForm: PelletsInformation provided by Rava.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM Data |
BASF Capron® 8202 NL Nylon 6 (Dry)
(discontinued **) Capron 8202 NL is an unfilled, low viscosity, non-lubricated nylon 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is available in natural, heat sta.. |
|||
Flexural Modulus | 2.82 GPa @Thickness 3.20 mm |
410 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical Lupox® GP1000A PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES Electrablend® POM CO Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and Medium ViscosityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 E2 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 E40 Availability: North AmericaForms: PelletsProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 L BK Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackTPCI# 9356102Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 L LE MB Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Lubricated, Heat Stabilized and Low ExtractablesAppearance: Colors AvailableTPCI# 7964102Information provide.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES HiFill® PA6 L UV (Dry) Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6 L N BK MB Nylon 6 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Fast Molding Cycle, Good Processability, Nucleated and LubricatedTPCI# 7970102Information provided by TP Co.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Techmer ES Plastiblend® PA6/6,6 109 L Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Copolymer and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.83 GPa @Thickness 3.20 mm |
410 ksi @Thickness 0.126 in |
Injection Molded; ASTM D790 |
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi.. |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Clariant Renol 6001 M2 Nylon 6, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Clariant Renol BR2029 Nylon 66, General Purpose, Black Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Clariant Renol PA211 Nylon 6, General Purpose Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | ASTM D790 |
Clariant Renol PA111BK S&P Nylon 66, General Purpose Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.83 GPa | 410 ksi | JIS-K-6740 |
Denka VINYKON R3102 PVC, R grade for hard extrusion A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |