Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was de.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)
(Unverified Data**) Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids... |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Polymer Resources AC-G10 Acetal Copolymer, 10% Glass Reinforced Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.62 - 10.7 GPa | 380 - 1550 ksi | Average value: 5.33 GPa Grade Count:7 |
Overview of materials for Polycarbonate/Polysulfone Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
BASF Capron® B85QP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.62 GPa @Thickness 3.17 mm |
380 ksi @Thickness 0.125 in |
|
KEP Kepital® F20 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ ABS-0502ARX Biocompatible, Antimicrobial ABS A biocompatible, high gloss injection molding grade of ABS for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KL004A Acetal Homopolymer LNP LUBRICOMP* KL004A is a compound based on Acetal Homopolymer resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU) Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 TL20 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated, Low Friction and Good Wear ResistanceUL File Number: E157318TPCI# 9740101Information provided by TP Compos.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Techmer ES Luriblend® PSU TL20 Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 1% Secant; ASTM D790 |
Washington Penn Medium Impact Copolymer 40% Talc Filled Talc-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug packaging requi.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D-790 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | 23°C, 50% RH; ASTM D790 |
Asahi Kasei Xyron® A0210 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
BASF Capron® B73ZP Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ISO 178 |
BASF Nypel® 2314 HS BK6 PA6 (Dry) Description: Nypel® 2314 HS BK6 is a black pigmented, low viscosity, heat stabilized, semi crystalline, injection molding compound based on recycled PA6 feedstocks. It also offers the following: go.. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
(Unverified Data**) Veradel A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to .. |
|||
Flexural Modulus | 2.62 GPa | 380 ksi | Tangent; ASTM D790 |
RheTech Products HP510-01UV 28% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Air ducts-structuralInterior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |