Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.48 GPa | 360 ksi | Tangent; ASTM D790 |
RheTech Products CC40P100-00 40% Calcium Carbonate Reinforced Polypropylene, Natural Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® XD 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses Features:Tough and durableResistant to cracking and chippingSolid, integral color3500+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantExcellent fabrication qualit.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
KYDEX® T MB High Impact Fire Rated Thermoforming Sheet with Microban® Antimicrobial Product Features:Substitute for FR-ABS sheet with competitive pricing but superior cost/performanceHigher breakage resistanceStandard thicknesses from 0.71 mm to 2.36 mmAmong the most rigid of thermoforming.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF14 IM4 HS L BKN 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Solvay Specialty Polymers Radel® R-7159 Polyphenylsulfone (PPSU) Radel® R-7159 polyphenylsulfone (PPSU) was developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical burn.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Europe-Africa-Middle East) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 LX Nylon 66 Availability: North AmericaForms: PelletsFeatures: Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Techmer ES Luriblend® PA6/6 TS18 Nylon 66 Availability: North AmericaForms: PelletsAdditive: PTFE + Silicone Lubricant (18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific) Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab.. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN213GL (COND, 50% RH) Nylon 66, 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1453 Calcium Carbonate Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1453 is a long term heat aging grade of 40% calcium carbonate filled homopolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Aaron Industries AAROPRENE® TFPP 2030 Talc Filled Polypropylene AAROPRENE® TFPP 2000 Series Talc Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFIPP 2020 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | Tangent; ASTM D790 |
RheTech Products CC40P100-01 40% Calcium Carbonate Reinforced Polypropylene, Black Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
PolyOne Edgetek® MP-1000 Modified PPO - Unreinforced
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3500B Description: Blow Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.48 GPa | 360 ksi | ASTM D790 |
Polimeri Europa SINKRAL L320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an .. |