Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.31 GPa | 335 ksi | Tangent; ASTM D790 |
RheTech Products G10P100-01 10% Glass Fiber Reinforced Polypropylene, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | Tangent; ASTM D790 |
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-UV1-D-[color]-1 Polycarbonate, UV-stabilized, Low Flow with Mold Release Polycarbonate, UV-stabilized, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources TP-GP1F Polybutylene Terephthalate, General Purpose, FDA-compliant Feedstocks Polybutylene Terephthalate, General Purpose, FDA-compliant FeedstocksProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPM1944 PC (Europe-Africa-Middle East) Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
PolyOne Geon™ SF M7010 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
PolyOne Geon™ SF M7020 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | RT; ASTM D-790-95 |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 (Europe-Africa-Middle East) LNP* Lubriloy* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP NX07354 PC+ABS (Asia Pacific) This is a PC/ABS compound, a good candidate for Laser Direct Structuring applications. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp XL004 Amorphous Polyamide LNP* Lubricomp* XL-4040 is a compound based on Amorphous Nylon, containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790 |
Styron CALIBREâ„¢ 302V-6 LD Polycarbonate Resin Overview: CALIBREâ„¢ 302V-6 LD HC18010009 Polycarbonate is an opalescent white extrusion-grade resin containing a proprietary light diffusion package that offers an excellent combination of light.. |
|||
Flexural Modulus | 2.31 GPa | 335 ksi | chs 0.05 in/min; ASTM D790 |
Diamond Polymers DIAMALOY 1418EF Polycarbonate/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |