Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 23.0 GPa | 3340 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)
(Unverified Data**) Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 1105-8002 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 1105-8205 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 1301-8517 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 20-0659 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 20-8171 Polyphthalamide, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 1105/CF/30/EM PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36EXP PPS - LINEAR LNP* LUBRICOMP* OCL36EXP is a compound based on Linear PPS containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include; Wear Resistant, Electrically Conductive. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | ISO 178 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA), 30% Carbon Fiber Ixef® 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than gla.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | ISO 178 |
Sumitomo Bakelite North America CF 9040A Carbon Fiber Reinforced Phenolic CF 9040A is a high strength carbon fiber phenolic molding compoundInformation provided by Sumitomo Bak North America, Inc. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | ASTM D790 |
Sumitomo Bakelite North America Epiall® 1904B-1 Short Glass Fiber Reinforced Epoxy Epiall 1904B-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided .. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | |
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc.. |
|||
Flexural Modulus | 23.0 GPa | 3340 ksi | DIN 53 457 |
Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber
(discontinued **) High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fan Blades, Brake Sleeves, Model Constructi.. |