Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.25 GPa | 326 ksi | ISO 178 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ISO 178 |
Radici Radilon® AHSX88 (dry) Nylon 66 Elastomer modified free conditioningInformation provided by Radici group. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HPX8R PC Copolymer (Asia Pacific) Very high flow specialty polycarbonate with outstanding processability and ductility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 o.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific) Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific) Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Asia Pacific) High flow PC+ABS material designed for local Pacific Automotive applications |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ASTM D790 |
PTS Trilac® ABS-HS6500 High Impact ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HP6NR PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | Superior Grade, 1st Grade |
Kazanorgsintez PC-007 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of extrusion and die-casting.Information Provided by Kazanorgsintez |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | |
Kazanorgsintez PC-075 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well .. |
|||
Flexural Modulus | 2.25 GPa @Thickness 3.17 mm |
326 ksi @Thickness 0.125 in |
ASTM D790 |
Global ABS-HI-121 High Impact ABS Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 2.25 GPa @Thickness 3.17 mm |
326 ksi @Thickness 0.125 in |
|
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ISO 178 |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-8002 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.0mm, V-2 @ 3.2mmExcellent balancing properties, Non-DPOExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV and audio housingElec.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2mm/min; ASTM D790 |
Kingfa FRHIPS-930 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, 5VA @ 2.6mmNon-DPO, high UV stabilityExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingPrinter, photocopier, fax machineElec.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ASTM D790 |
SABIC Innovative Plastics NORYL SE100V PPE+HIPS (Asia Pacific) |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ASTM D 790 |
Cossa Polimeri ESTABLEND PSA 7600 PC / ASA Blend Polycarbonate and acrylonitrile styrene acrylate blendGood light resistance, good impact resistance, high heat resistance, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | Secant; ISO 178 |
ExxonMobil Exxtral™ LNU 012 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good heat resistance and good surface finish designed for fast injection molding of large electrical appliance parts.Availability.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 15mm/min; ASTM D790 |
Denka MALECCA K-300 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | ISO 178 |
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Flexural Modulus | 2.25 GPa | 326 ksi | |
Kazanorgsintez PC-075D Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for manufacture of optical products by method of die-casting (including CD, DVD, and other discs), as well .. |