Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM D790 |
PolyOne Maxxam™ PPH-10G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 2.21 - 2.34 GPa | 321 - 339 ksi | ASTM D790 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® EXL1493T PC Copolymer Lexan* EXL1493T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance, with mold release. This resin offers excellent low temperature (-3.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa.. |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(22) 22 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East) Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Asia Pacific) Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Europe-Africa-Middle East) Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTPM307 ASA+PC (Europe-Africa-Middle East) XTPM307 is a high heat resistant PC/ASA with improved processing stability over HRA150. Typical values measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10FR-(V18) 18 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa @Thickness 3.17 mm |
321 ksi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp JL003 PES LNP* Lubricomp* JL003 is a compound based on Polyethersulfone resin containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Asia Pacific) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the A.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ISO Data |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM Test |
BASF Ultramid® 8253 HS PA6 (Dry) Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM Value |
BASF Capron® 8253 Impact Modified Nylon 6 (Dry)
(discontinued **) Capron 8253 is an unfilled type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Capron 8253 HS) and/or pigmented versions.. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® EXL1433T PC Copolymer Lexan* EXL1433T polycarbonate (PC) siloxane copolymer resin is a UV stabilized transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1001L Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1001L is an unreinforced, impact modified polyphthalamide (PPA) resin that exhibits exceptional impact strength at temperatures ranging from room temperature to as low as -40°F (-40°C), .. |
|||
Flexural Modulus | 2.21 GPa | 321 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xylex FXY391DF PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy in Diffusion Visual fx. This grade is compliant with US FDA/European food contact regulations. Color package may influence performance.This data was supplied by SABIC-IP for the E.. |