Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products FRP300-01 20% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products HP514-393 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 110D Medium Dark Pewter Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products HP514-447 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 9902 Very Dark Gray Applications: Interior trimCenter consolesFuse panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Oxford Polymers INJ-FR Glass Fiber Reinforced ABS, Flame Retardant Glass Fiber Reinforced ABS, Flame RetardantInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
RheTech Products HP514-00UV 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.21 - 7.86 GPa | 320 - 1140 ksi | Average value: 5.37 GPa Grade Count:15 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant". Each property range of valu.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Solvay Specialty Polymers Supradel® HTS-2601 High Temperature Sulfone Resin
(discontinued **) Supradel HTS-2601 is a high-temperature high-performance amorphous sulfone polymer designed as a base resin for reinforced thermoplastic products. This exceptional thermal performance is available i.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | Tangent; ASTM D790 |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Techmer ES HiFill® PP 0159 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.21 - 2.62 GPa | 320 - 380 ksi | ASTM D790 |
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | |
Zylog Hipolyene® 8021 M Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 2.21 GPa @Thickness 6.40 mm |
320 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy ABS-polycarbonate alloys for High service temperature applications.Information provided by Bhansali |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D-790 |
Axiall 8150 Rigid PVC, Extrusion & Molding Georgia Gulf 8150 is a special purpose rigid PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChemical Resista.. |
|||
Flexural Modulus | 2.21 GPa | 320 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFIPP 2010 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 2.21 GPa @Thickness 6.40 mm |
320 ksi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-20P ABS Sheet Extrusion Grade ABS Pipe GradeInformation provided by Bhansali |
|||
Flexural Modulus | 2.21 GPa @Thickness 6.40 mm |
320 ksi @Thickness 0.252 in |
ASTM D790 |
Bhansali Engineering Abstron IM-11 ABS Injection Molding Grade High Impact, High Rigidity, High Fatigue, Low Flow, PaintableInformation provided by Bhansali |