Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.20 GPa | 319 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Asia Pacific) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 2.20 - 3.20 GPa | 319 - 464 ksi | ASTM D790 |
Prodways PLASTCure Cast 200 3D Printing Polymer Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178, ASTM D790 |
Nilit Nilitop BT N Unfilled, Nucleated PBT Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
Nilit FRIANYL B63 TF30 Nylon 6 for injection molding, 30% PTFE lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 2.20 GPa @Temperature 23.0 °C |
319 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB SCANTEC PC S60R Polycarbonate Information provided by Polykemi AB |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2mm/min; ASTM D790 |
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2mm/min; ASTM D790 |
Kingfa LONOY 1200 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2mm/min; ASTM D790 |
Kingfa LONOY 1300 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | |
Lehmann & Voss LUVOCOM® 1850/PL/15/BK PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Parts for electric and electro.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® ABS 640 Injection Molding Grade Lustran® ABS 640 has high impact strength and is injection molding grade. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 3 points and 1 mm/min; ISO 178 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX0844 PPE+HIPS (Europe-Africa-Middle East) NORYL PX0844 is an unfilled standard material with a Vicat B/120 of 125°C according ISO306. NORYL PX0844 offers high heat resistance and consistant processability. Typical |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
Polyram RamOfin PPH343T4BK10 Polypropylene, 20% Mineral Filled 20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | >= 2.20 GPa | >= 319 ksi | ASTM-D790 |
Polyram RamTough RZ222 Polycarbonate, Injection Molding Polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1434 Couple Mica In Copolymer Polypropylene (25% Mineral Filled) DescriptionPolyfort® FPP 1434 is a 25% coupled mica copolymer polypropyleneInformation provided by A. Schulman. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D 790 |
Cossa Polimeri ESTAPROP 1040 V2 H Flame Retardant Polypropylene PP homopolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® GL3200 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
Chem Polymer Chemlon 104 Nylon 66, Medium Impact GP A medium viscosity, impact-modified, lubricated nylon 66 exhibiting improved toughness.Data provided by the manufacturer, Chem Polymer. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, DAM Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ISO 178 |
Polyplastics Duracon® NW-02 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Modulus | 2.20 GPa | 319 ksi | ASTM D790 |
SABIC Innovative Plastics Lexan® MHL1110 PC (Asia Pacific) |