Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
PolyOne Nymax™ 1308 A HS Natural Polyamide 66 (Nylon 66) The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range o.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | Tangent; ASTM D790 |
RheTech Products T20P200-01BG 20% Talc Reinforced Polypropylene Copolymer, General Purpose Black, Blow Molding Grade Applications: HVAC ductsSeat backsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 0.1 in/min; ASTM D790 |
Ineos Nova Zyntar® 7001 High Performance Flame Retardant Polystyrene
(discontinued **) Super high flow, Reduced processing temperatures, Reduced processing time, Improved aesthetics, Custom colorsApplications: Injection molding, Gas-assist injection molding, Hard to fill cavities, suc.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Global CPP-120 20% CaCO3 Filled, Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 1.93 GPa @Thickness 3.17 mm |
280 ksi @Thickness 0.125 in |
ASTM D790 |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PCT1000 PC/PET Alloy PC/PET alloy with outstanding chemical resistance and impact strengthAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | secant; ASTM D790 |
Spartech DP5120 Talc Filled Homopolymer Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Spartech Royalite R57 FR/ABS Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Spartech Weather-Pro Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® BM-0320 J ABS, Unreinforced Heat resistantInformation provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Samsung Cheil Industries Starex® WR-9140 General Purpose ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF V1000 PA 66 LNP THERMOTUF* V1000 is a compound based on Nylon resin. Added features of this material include: High Impact. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Techmer ES HiFill FR® HIPS FR-1 Availability: North AmericaForms: PelletsFeatures: Flame RetardantRoHS Compliance: RoHS CompliantInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® 625L Nylon 6/6 (DAM) Polifil® NYLON 6/6 combines good abrasion and chemical resistance.Applications: ValvesBearingsBearing casesStandard processing techniques are applicable. Information provided by The Plastics Group... |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1427 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 1247 is a 25% mineral filled copolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® GFRMPPCC-10 10% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 5143S Homopolymer Polypropylene Homopolymer for Extrusion Sheet and Thermoforming Applications Formolene® 5143S is a higher melt flow homopolymer designed for light weighting of components. Its very high stiffness enables reducti.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Chesterton ARC S1 General purpose coating Description: An advanced polymer composite formulated to protect metal surfaces from corrosion and chmical attack. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrink.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Ensinger Hydex™ 202 Rigid Polyurethane (PU) Hydex™ 202 is a totally rigid polyurethane resin that exhibits a broad range of chemical resistance, as well as superior impact and excellent mechanical properties. It can be used for any mechanic.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Entec Hylac® EX18 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
3D Systems Accura® accuGen™ Nd Plastic for SLA® Systems Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® Viper si2™, 3500, 5000 & 7000 systems.Typical ApplicationsMulti-purpose mode.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem F350HC2 High Crystallinity Homopolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive, AppliancesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | ASTM D790 |
Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 1.93 GPa @Temperature 120 °C |
280 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Flexural Modulus | 1.93 - 2.41 GPa | 280 - 350 ksi | Average value: 2.18 GPa Grade Count:25 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 1.93 GPa | 280 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |