Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P6-9900-0570 Unfilled, Flame Retardant, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Yield 30 %
30 %
ASTM D638
Flexural Strength 38.6 MPa
5600 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.14 J/cm
4.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C
240 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
ASTM D648
Flammability, UL94 V-0
V-0
0.0279 in thickness