Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Resinoid 1340 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 20-7343 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105/XCF/25 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-0699 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-7141 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific) LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, DRY Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UCL16AS PPA (Europe-Africa-Middle East) Internally lubricated Polyphthalamide compound, containing Carbon Fiber and PTFE. Added features include Heat Stabilized |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® BR111BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111BL Ryton® BR111 is a black-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outs.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-220BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.Features: Good S.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Sumitomo Bakelite North America RX® 630 Fiberglass Reinforced Phenolic RX 630 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North America. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
Solvay TECHNYLSTARâ„¢ SX 218 L2 V60 Black JA6A PA6, 60% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 60% of glass fiber, heat and UV stabilized, characterized by a high fluidity of the melt, for injection molding.Available in: Europe Product Applic.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX12419 PA 6 LNP* THERMOCOMP* PX12419 is a compound based on Nylon 6 containing Carbon Fiber. Added features of this grade include: Electrically Conductive. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | DIN 53 457 |
Albis Plastics Tedur® L 9523 PPS, 60% Glass Fiber/Mineral Extremely Rigid, Excellent Surface Finish, Metallization w/o Base Coating. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Insulating Equipment, Reflectors and Fitting.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Resinoid 1323 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ASTM D790 |
Resinoid 1324 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Verton RV00CESP PA6.6 (Europe-Africa-Middle East) LNP* VERTON* RV00CESP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Verton RV00CEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | |
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Flexural Modulus | 19.0 GPa | 2760 ksi | ISO 178 |
LNP Verton™ UF-700-12 Polyphthalamide, Long Glass Fiber Filled
(discontinued **) LNP™ Verton™ UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized.Information provided by LNPThis dat.. |