SABIC Innovative Plastics LNP Verton RV00CESP PA6.6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics LNP Verton RV00CESP PA6.6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* VERTON* RV00CESP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
ISO 1183
Water Absorption 0.90 %

@Temperature 23.0 °C,
Time 86400 sec
0.90 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 279 MPa
40500 psi
5 mm/min; ISO 527
Tensile Strength, Yield 281 MPa
40800 psi
5 mm/min; ISO 527
Elongation at Break 1.7 %
1.7 %
5 mm/min; ISO 527
3.0 %
3.0 %
Flexural Strain, 2 mm/min; ISO 178
Elongation at Yield 1.7 %
1.7 %
5 mm/min; ISO 527
Tensile Modulus 21.6 GPa
3130 ksi
1 mm/min; ISO 527
Flexural Yield Strength 418 MPa
60600 psi
2 mm/min; ISO 178
Flexural Modulus 19.0 GPa
2760 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 52.0 kJ/m²

@Temperature 23.0 °C
24.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 95.0 kJ/m²

@Temperature 23.0 °C
45.2 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 255 °C
491 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af