Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 13.3 GPa @Temperature 23.0 °C |
1930 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | |
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both in.. |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Flexural Modulus | 13.31 GPa | 1930 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP VERTON RV00AE PA 66 LNP* VERTON* RV00AE is a compound based on Nylon 66 containing 50% Long Glass Fiber. Added features of this grade include: Easy Molding, Structural. |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | ASTM D790 |
Plenco 08225 Polyester BMC, Compression Molded PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding propert.. |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | ASTM D790 |
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo. |
|||
Flexural Modulus | 13.3 GPa | 1930 ksi | ISO 178 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |